CaO-Al_2O_3-SiO_2三元系中两相区边界上活度的计算
蔡文娟;周国治
北京钢铁学院;北京钢铁学院
CALCULATION OF ACTIVITIES ON TWO-PHASE REGION BOUNDARIES IN CaO-Al_2 O_3 -SiO_2 TERNARY SYSTEM
by CAI Wenjuan; ZHOU Guozhi(Beijing University of Iron and Steel Technology)(Manuscript received 16 July; 1985; revised manuscript 14 May; 1986)
引用本文:

蔡文娟;周国治. CaO-Al_2O_3-SiO_2三元系中两相区边界上活度的计算[J]. 金属学报, 1987, 23(5): 480-485.
, . CALCULATION OF ACTIVITIES ON TWO-PHASE REGION BOUNDARIES IN CaO-Al_2 O_3 -SiO_2 TERNARY SYSTEM[J]. Acta Metall Sin, 1987, 23(5): 480-485.

全文: PDF(478 KB)  
摘要: 本文对CaO-Al_2O_3-SiO_2三元系中两相区边界上的活度作了计算。计算结果被表示为结线与棱边的交点成分和活度之间的关系曲线,这种表示法可以很方便地直接读取某组元的活度.本计算法可以推广到其它三元系中.
Abstract:Calculation of activities on the two-phase region boundaries in CaO-Al_2O_3-SiO_2 ternary system has been carried out. Relationships between the activities of components and the composition of intersection of tie-line and composition edges along two-phase boundaries have also been presented, upon which the activities may easily be read. This method can also be used in other ternary systems.
收稿日期: 1987-05-18     
1 Chou K C(Zhou Guozhi) (周国治), Elliott J F. Chemical Metallurgy-A Tribute to Carl Wagner, New York: AIME, 1981: 195
2 周国治,蔡文娟,马美娟。见:第三届全国熔盐化学和电化学会议论文集,三元系中两相区边界上的活度之间的关系,1985
3 周国治,蔡文娟,马美娟.见:第三届全国熔盐化学和电化学会议论文集,三元系中两相区边界上的活度与t函数之间的关系,1985
4 Choudary U V, Chang Y A. Metall Trans, 1976; 7B: 655
5 Wang Zhichang (王之昌), Zhou Guozhi (周国治), Scientia Sinica, 1984; 27(12) : 1328-1338
6 Zhou Guozhi (周国治). Scientia Sinica, 1978; 21(5) : 601
7 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking, Vol. Ⅱ, Reading Mass: Addison-Wesley, 1963: 592-59