| 40CrNiMoA钢Ⅱ型试样的腐蚀疲劳 |
| 褚武扬;肖纪美;赵予生 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| CORROSION FATIGUE CRACK INITIATION IN A MODE Ⅱ NOTCH SPECIMEN |
| by CHU Wuyang; XIAO Jimei (C. M. Hsiao); ZHAO Yusheng (Beijing University of Iron and Steel Technology)(Manuscript received 27 August; 1985) |
引用本文:
褚武扬;肖纪美;赵予生. 40CrNiMoA钢Ⅱ型试样的腐蚀疲劳[J]. 金属学报, 1987, 23(5): 396-402.
,
,
.
CORROSION FATIGUE CRACK INITIATION IN A MODE Ⅱ NOTCH SPECIMEN[J]. Acta Metall Sin, 1987, 23(5): 396-402.
1 Kocanda S. Fatigue Failure of Metals, Warsaw: Sijthoff and Noordhoff international publishers, 1978 2 Chu W Y (褚武扬), Hsiao C M. (肖纪美), Liu TH (刘天化). Fatigue Eng Mater Struct 1984; 7: 279 3 张统一,褚武扬,肖纪美,李英,金属学报,1986;22:A349. 4 中国航空研究院主编.应力强度因子手册,科学出版社,1981;122 5 Wang YB(王燕斌),chu WY(褚武扬),Hsiao CM(肖纪美).Scr Metall,1985;19:1161 6 张统一,褚武扬,肖纪美.中国科学,A,1986;(3) :316# |
|