| 低碳钢的相间沉淀 |
| 石德珂;宋晓平 |
| 西安交通大学;西安交通大学 |
|
| INTERPHASE PRECIPITATION IN LOW CARBON STEELS |
| by SHI Deke; SONG Xiaoping (Xi'an Jiaotong University)(Manuscript received 27 December; 1985; revised manuscript 15 September; 1986) |
引用本文:
石德珂;宋晓平. 低碳钢的相间沉淀[J]. 金属学报, 1987, 23(5): 386-390.
,
.
INTERPHASE PRECIPITATION IN LOW CARBON STEELS[J]. Acta Metall Sin, 1987, 23(5): 386-390.
1 Honeycombe R W K. Met Sci, 1980; 14: 201 2 石德珂,柴惠芬 谈育煦,胡奈赛.钢中粒状贝氏体的组织与性能,西安交通大学科技报告,1978-063 3 俞德刚,郑经紘,梁振峰,沈甫法。金属学报,1983;19:A369 4 李承基.金属热处理学报,1984;5(2) :1 5 #12 6 Swanson WD, Parr J G. J Iron Steel Inst, 1964; 202: 104 7 Roberts M J. Metall Trans, 1970; 1: 3287 8 Wilson E A. Scr Metall, 1978; 12: 961 9 Massalski TB. Metall Trans, 1984; 15A: 421 10 Aaronson HI, Plichta MR, Franti G W, Russell K C. Metall Trans, 1978; 9A:363o |
|