| 蝶状马氏体的复生机制 |
| 贡海;谷南驹 |
| 大连铁道学院;河北工学院 |
|
| FORMATION MECHANISM OF BUTTERFLY MARTENSITE |
| by GONG Hai (Dalian Institute of Railway); GU Nanju (Hebei Technological Institute; Shijiazhuang)(Manuscript received 28; February;1986) |
引用本文:
贡海;谷南驹. 蝶状马氏体的复生机制[J]. 金属学报, 1987, 23(5): 374-379.
,
.
FORMATION MECHANISM OF BUTTERFLY MARTENSITE[J]. Acta Metall Sin, 1987, 23(5): 374-379.
1 梅本実,田村今男.水曜会誌,1980;119:281 2 贡海,苏东升.金属热处理,1983;(1) :32 3 纪芬,贡海.理化检验(物理分册),1985;21(5) :11 4 梅本実,渡井康之,田村今男.日本金属学会会誌,1980;44:453 5 Brook R, Entwisle A R. J Iron Steel Inst. 1965; 203: 905 6 Umemoto M, Tamura I. Proc of ICOMAT-79, Cambridge (USA), 1979: 53 7 Tamura I. Proc of ICOMAT-76, Kobe(Japan), 1976: 5 |
|