| 金属间化合物ZrAl_3的内部结构对晶体形态的影响 |
| 舒震;G.J.Davies |
| 湖南大学;英国Sheffield大学 |
|
| ON THE INFLUENCE OF INTERNAL STRUCTURE OF INTERMETALLIC COMPOUND ZrAl_3 ON ITS MORPHOLOGY |
| by SHU Zhen (Hunan University); G.J.DAVIES (University of Sheffield; U. K.) (Manuscript received 3 May; 1984; revised manuscript 29 June; 1986) |
引用本文:
舒震;G.J.Davies. 金属间化合物ZrAl_3的内部结构对晶体形态的影响[J]. 金属学报, 1987, 23(4): 267-273.
,
.
ON THE INFLUENCE OF INTERNAL STRUCTURE OF INTERMETALLIC COMPOUND ZrAl_3 ON ITS MORPHOLOGY[J]. Acta Metall Sin, 1987, 23(4): 267-273.
1 Hartman P, Perdok W G. Acta Crystallogr. 1955; 8: 49, 521 2 Hartman P. In:Hartman P ed., Structure and Morphology in Crystal Growth: An Introduction, Amsterdam: North-Holland, 1973; 367 3 Felius R O. Structure morphology of Rutile and Trirutile Type Crystals, Dutch Efficiency Bureau, Pijnacker, 1976 4 Hartman P. J Cryst Growth, 1968; 2: 385 5 Hartman P, Bennema P. J Cryst Growth, 1980; 49: 145 6 Hartman P.J Cryst Growth, 1980; 49: 157, 166 7 Tassoni D, Riquet J P, Durand F. Acta Crystallogr, A, 1980; 36: 420 8 Hamer R, Tassoni D, Riquet J P, Durand F. J Cryst Growth, 1981; 51: 493 9 Brauer G. Z Anorg Allg Chem, 1939; 242: 1 10 Shu Zhen, Davies G J. J Cryst Growth, 1983; 64: 407 11 Fink W L, Willey L A. Trans AIME, 1939; 133: 69 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|