| Au-Cu合金择优溅射机制的一个新观点 |
| 李日升 |
| 中国科学院金属研究所 |
|
| A NEW VIEWPOINT ON MECHANISM OF PREFERENTIAL SPUTTERING OF Au-Cu ALLOYS |
| by LI Risheng (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 30 December; 1985; revised manuscript 15 June; 1986) |
引用本文:
李日升. Au-Cu合金择优溅射机制的一个新观点[J]. 金属学报, 1987, 23(4): 253-261.
.
A NEW VIEWPOINT ON MECHANISM OF PREFERENTIAL SPUTTERING OF Au-Cu ALLOYS[J]. Acta Metall Sin, 1987, 23(4): 253-261.
1 Behrisch R. Sputtering by Particle Bombardment 1 and 2, Berlin: Springer, 1981 and 1983 2 Wehner G K. In: Czanderna A W ed. Methods of Surface Analysis, Amsterdan: Elservier, 1975: 5 3 Betz G. Surf Sci, 1980; 92; 283 4 Kelly R. Surf Sci, 1980; 100: 85 5 Li R S(李日升), Koshikawa T, Goto K.Surf Sci, 1982; 121: L 561 6 Patterson W L, Shirn G A. J Vac Sci Technol, 1967; 4: 343 7 Pickering H W. J Vac Sci Technol, 1976; 13: 618 8 Ho P S 何兆中. Surf Sci, 1978; 72: 253 9 Koshikawa T, Goto K, Saeki N Shimizu R, Sugata E. Surf Sci 1979; 79: 461 10 Okutani T, Shikata M, Shimizu R. Surf Sci, 1980; 99: L410 Kang H J,Shimizu R, Okutani T. Surf Sci, 1982; 116: L173 11 Swartzfager D G, Ziemecki S B, Kelley M J. J Vac Sci Technol, 1981; 19: 185 12 Farber W, Betz G, Braun P. Nucl Instrum Methods, 1976; 132: 351 13 Tompkins H G. J Vac Sci Technol, 1976; 16: 778 14 Ichimura S, Shimizu R, Ikuda T. In: Johari O, Scanning Electron Microscopy, AMF O'Hare,IL, 1981 15 LiR S (李日升),Koshikawa T, Goto K,In: Proc Ann Meeting Japan Society of Applied Physics, 1981: 254 16 Ho P S, Lewis J E, Wildman H S, Howard J K. Surf Sci, 1976; 57: 393 17 Kelly R. Surf Interface Anal, 1985; 7: 1 18 Kelly R.私人通讯,1984 19 Li R S (李日升), Koshikawa T. Surf Sci 1985; 151: 459 20 See, For example, Okamoto P R, Rehn L E. J Nucl Mater, 1979; 83: 2, and references therein 21 Li R S (李日升), Tu L X (屠礼勋), Sun Y Z (孙玉珍). Surf Sci, 1985; 163: 67. 22 LiRS (李日升), TuLX (屠礼勋), Sun Y Z(孙玉珍). Appl Surf Sci, 1986; 26: 77 23 Betz G, Braum P, Farber W. J Appl Phys, 1977; 48: 1404 24 Nakamura H, Morita K, Itoh N. Nucl Instrum Methods, 1981; 191: 119 25 Holloway P H, Bhattacharya R S. J Vac Sci Technol, 1982; 20: 444 26 Itoh N, Morita K. Radiat Eff, 1984; 80: 163 27 Andersen H H, Stenum B, Sorensen T, Whitlow H J. Nucl Instrum Methods, 1983; 209/210: 487 28 Sigmund P, Oliva A, Falcone G. Nucl Instrum Methods, 1982; 194: 541 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|