| 蔡开科;刘新华 |
| 北京钢铁学院;北京钢铁学院 |
|
| ON THE COARSE INCLUSIONS IN CONTINUOUS CASTING STRANDS |
| CAI Kaike; LIU Xinhua(Beijing University of Iron and Steel Technology) (Manuscript received 28 September; 1985; revised manuscript 8 April; 1986) |
引用本文:
蔡开科;刘新华. 连铸坯大型夹杂物的研究[J]. 金属学报, 1987, 23(3): 291-292.
,
.
ON THE COARSE INCLUSIONS IN CONTINUOUS CASTING STRANDS[J]. Acta Metall Sin, 1987, 23(3): 291-292.