| Fe-Co-Si-B非晶态溅射薄膜的热稳定性 |
| 冯群;冯敏英;王亦忠;王震西 |
| 中国科学院物理研究所;中国科学院物理研究所;中国科学院物理研究所;中国科学院物理研究所 |
|
| THERMAL STABILITY OF AMORPHOUS Fe-Co-Si-B THIN FILM PREPARED BY SPUTTERING |
| FENG Qun; FENG Minying; WANG Yizhong; WANG Zhenxi(Institute of Physics; Academia Sinica; Beijing) (Manuscript received 16 August; 1985; revised manuscript 6 May; 1986) |
引用本文:
冯群;冯敏英;王亦忠;王震西. Fe-Co-Si-B非晶态溅射薄膜的热稳定性[J]. 金属学报, 1987, 23(3): 288-290.
,
,
,
.
THERMAL STABILITY OF AMORPHOUS Fe-Co-Si-B THIN FILM PREPARED BY SPUTTERING[J]. Acta Metall Sin, 1987, 23(3): 288-290.