| 用正电子湮没方法测定Nd在Fe中的固溶度 |
| 王蕴玉;刘年庆;田中卓;常香荣 |
| 中国科学院高能物理研究所;中国科学院高能物理研究所;北京钢铁学院;北京钢铁学院 |
|
| DETERMINITION OF THE SOLUBILITY OF NEODYMIUM IN IRON BY POSITRON ANNIHILATION |
| WANG Yunyu; LIU Nianqing(Institute of High Energy Physics; Academia Sinica; Beijing) TIAN Zhongzhuo; CHANG Xiangrong(Beijing university of lron and Steel Technology) (Manuscript received 24 October 1985; revised manuscript 5 July; 1986) |
引用本文:
王蕴玉;刘年庆;田中卓;常香荣. 用正电子湮没方法测定Nd在Fe中的固溶度[J]. 金属学报, 1987, 23(3): 285-287.
,
,
,
.
DETERMINITION OF THE SOLUBILITY OF NEODYMIUM IN IRON BY POSITRON ANNIHILATION[J]. Acta Metall Sin, 1987, 23(3): 285-287.
1 王蕴玉,刘年庆,常香荣,田中卓,吕荣邦,肖纪美,曹必松.核技术1982;6:33 2 曹必松,王蕴玉,张天宝,田中卓,常香荣.核技术1982;6:56 3 Dlubeh G. Phys Status Solidi (a), 1979; 55: 509 |
|