Please wait a minute...
金属学报  1987, Vol. 23 Issue (3): 257-261    
  论文 本期目录 | 过刊浏览 |
NaCl-KCl熔盐中电解渗Al电极过程的研究
马樟源;徐之强;曹铁梁;石声泰
中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所;江西大学82届毕业生
ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH
MA Zhangyuan; XU Zhiqiang; CAO Tieliang; SHI Shengtai (Shih Shing-Tai)(Shanghai Institute of Metallurgy; Academis Sinica) (Manuscript received 22 July; 1984; revised manuscript 26 November; 1985)
引用本文:

马樟源;徐之强;曹铁梁;石声泰. NaCl-KCl熔盐中电解渗Al电极过程的研究[J]. 金属学报, 1987, 23(3): 257-261.
, , , . ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH[J]. Acta Metall Sin, 1987, 23(3): 257-261.

全文: PDF(350 KB)  
摘要: 作者在熔盐中研究了Al的氧化/还原电位,作图法求得为-1.122V,阳极溶解为Al→Al~(3+)+3e用稳态法研究阴极过程,对一些离子的析出电位、AlCl_4~-扩散系数和Al~(3+)还原反应动力学参数进行了测量和讨论。
Abstract:The standard oxidation/reduction potential of Al including its valence state in fused salt was examined, The anodic dissolution of Al can be shown by the equation Al→Al~3+3e. The standard oxidation/reduction potential of Al in fused salt is-1.122V as obtained by graphical method. Cathodic process has been investigated by means of steady state method. Separate potentials of some ions, the coefficient of diffusion ,of AlCl_4~- ion and kinetic constants of Al ion reduction have been meastured and discussed.
收稿日期: 1987-03-18     
1 石声泰 (Shin S T). In: Rapp R A ed., High Temperature Corrosion, NACE-6, 1983: 460
2 石声泰.中国腐蚀与防护学报,1981;1(3) :1-7
3 石声泰,冯明仁,曹铁梁,马樟源,张彩玲.中国腐蚀与防护学报,1981;1(4) :1-7
4 Shin S T (石声泰), Feng M R (冯明仁), Cao T L (曹铁梁), Zhang C L (张彩玲). In: Metallic Corrosion, Proceedings 8th International Congress on Metallic Corrosion, 1981, Vol. Ⅱ, Deutsche Gesellschaft fur Chemisches Apparalewesen e. v. Frankfurt am Main, 1981: 1127
5 Winter D G, Strachan A M. In: Jones M J. Advances in Extractive Metallurgy, An Int. Symp. Organized by the Institution Metallurgy, London: Inst. Mining and Metall., 1977: 177