| Al-Mg-Sm三元相图的400℃等温截面 |
| 郑朝贵;陈立翀;叶于浦 |
| 北京大学化学系;北京大学化学系;北京大学化学系 |
|
| PHASE EQUILIBRIA IN Al-Mg-Sm SYSTEM AT 400℃ |
| ZHENG Chaogui; CHEN Lichong; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 15 July; 1985; revised manuscript 26 May. 1986) |
引用本文:
郑朝贵;陈立翀;叶于浦. Al-Mg-Sm三元相图的400℃等温截面[J]. 金属学报, 1987, 23(3): 253-256.
,
,
.
PHASE EQUILIBRIA IN Al-Mg-Sm SYSTEM AT 400℃[J]. Acta Metall Sin, 1987, 23(3): 253-256.
1 Hansen M. Constitution of Binary Alloys, New Work: McGraw-Hill, 2nd Edition, 1958: 106 2 Iandelli A. National Physical Laboratory Symposium No. 9: The Physical Chemistry of Metallic Solution and Intermetallic Compounds, Vol. 1, London: Her Majesty's Stationary Office, 1959: 369-379 3 #12 4 郑朝贵,陈立翀,田曙坚,叶于浦.无机化学,1986;2(2) :80 5 Buschow K H J. J Less-Common Met, 1971; 24: 117 6 Buschow K H J. J Less-Common Met, 1965; 8: 75 7 Buschow K H J. Philips Res Rep, 1965; 20(1) : 15 8 Mondolfo L F. Aluminum Alloys: Structure and Properties, London-Boston, Butterworths, 1976; 376 9 Castcels F J. J Less-Common Met, 1967; 13: 370 10 郑朝贵,洪学韵,钱久信,叶于浦.中国稀土学报.1984;1(2) :78 11 #12 12 #12 13 #12 14 郑朝贵,吴有余,钱久信,叶于浦.金属学报,1986;22(2) :B638 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|