| 氢在奥氏体不锈钢应力腐蚀中的作用 |
| 乔利杰;褚武扬;肖纪美 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| ROLE OF HYDROGEN IN STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEEL IN BOILING MgCl_2 SOLUTION |
| QIAO Lijie; CHU Wuyang; XIAO Jimei (Beijing University of Iron and Steel Technology) (Manuscript received 11 April; 1985; revised manuscript 19 December; 1985) |
引用本文:
乔利杰;褚武扬;肖纪美. 氢在奥氏体不锈钢应力腐蚀中的作用[J]. 金属学报, 1987, 23(3): 228-233.
,
,
.
ROLE OF HYDROGEN IN STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEEL IN BOILING MgCl_2 SOLUTION[J]. Acta Metall Sin, 1987, 23(3): 228-233.
1 褚武扬编著.氢损伤和滞后断裂,冶金工业出版社,1984,(即将出版) 2 姚京,褚武扬,肖纪美。金属学报,1984;20:A124 3 Wilde B E, Kim C D. Corrosion, 1972; 28: 350 |
|