| 原粉末颗粒边界碳化物的研究 |
| 李慧英;胡本芙;章守华 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| STUDY OF PREVIOUS POWDER-PARTICLE BOUNDARY CARBIDES |
| LI Huiying; HU Benfu; ZHANG Shouhua (Beijing University of Iron and Steel Technology)(Manuscript received 21 April; 1985) |
引用本文:
李慧英;胡本芙;章守华. 原粉末颗粒边界碳化物的研究[J]. 金属学报, 1987, 23(2): 212-250.
,
,
.
STUDY OF PREVIOUS POWDER-PARTICLE BOUNDARY CARBIDES[J]. Acta Metall Sin, 1987, 23(2): 212-250.
1 Ingesten N G, Warren R, Winberg L. In: Byunetaud R, et al. eds. High Temperature Alloys for Gas Turbines, 1982 Proc. of a Conf. Held in Liege Belgium, 4-6 October 1982 2 Tien J K, Boesch W J, Howson T E, Castledine W B. P/M Superalloys Aerospace Materials for the 1980's A metal Powder Report Conf., Zurich, Switzerland, Nov. 1980 3 Dahlen M, Ingesten N G, Fischmeister H. Modern Developments in Powder Metallugy. Vol. 14. 1981. , 3-14 4 Dahlen M, Fischmeister H. In: Tien J K, ed. Prpc. 4th Int. Superalloy Symp., Seven Springs. 21-25 Sept. 1980. Ohio: ASM, 449-454 5 Aubin C, Davidson J H, Trotticr J P. In: Tien J K, ed. Proc. 4th International Superalloys Sy-mposium, 21-25 Sept. 1980, Ohio: ASM, 345-354 6 Menzies R G. Bricknell R.H. Philos Mag A 1980; 42: 493-508 7 胡本芙,李慧英,章守华,金属学报,1987;23:B95 8 Podob M T. Modern Developments in Powder Metallugy. Vol. 11, 1978, 25-44 9 Domingue J A, Boesch W J, Radavich J F. In: Tien J K, ed. Proc. 4th Int. Superalloy Symposium. Seven Springs, 21-25 Sept. 1980, Ohio: ASM, 335-344 10 章守华主编 合金钢,冶金工业出版社,1980 11 李慧英,胡本芙,章守华,(待发表) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|