| 金属玻璃Zr_(75.9)Ni_(24.1)的结晶动力学特性 |
| 张其瑞;曹致玉;H.C.Freyhardt |
| 中国科学技术大学物理系;中南工业大学数理系;联邦德国G(?)ttingen大学金属物理研究所 |
|
| CRYSTALLIZATION KINETICS OF THE METALLIC GLASS Zr_(75.9)Ni_(24.1) |
| ZHANG Qirui(Department of Physics; University of Science and Technology of China; Hefei); CAO Zhiyu (Cental South University of Technology;Changsha); FREYHARDT Herbert C. (Institut far Metallphysik;Universitat Gottingen; FRG)(Manuscript received 15 June; 1985; revised manuscript 25 March; 1986) |
引用本文:
张其瑞;曹致玉;H.C.Freyhardt. 金属玻璃Zr_(75.9)Ni_(24.1)的结晶动力学特性[J]. 金属学报, 1987, 23(2): 206-211.
,
,
.
CRYSTALLIZATION KINETICS OF THE METALLIC GLASS Zr_(75.9)Ni_(24.1)[J]. Acta Metall Sin, 1987, 23(2): 206-211.
1 张其瑞,Freyhardt H C.低温物理,1984;6:93 2 Zhang Q R, Kerbs H U, Freyhardt H C. In:Eckern V, Schmid A et al. eds. Proc. 17th Int. Conf. on Low Temperature Physics (Contributed papers). Amsterdam: North-Holland, 1985, 1313 3 Zhang Q R, Krebs H U, Freyhardt H C. In: steeb S, et al. eds. Proc. 5th Int Conf. on Rapidly Quenched Metals. Amsterdam: North-Holland 1985, 707 4 Cao Z Y, Fritsch H U, Bergmann H W. Thermochim Acta, 1985; 83: 23-28 5 Cao Z Y, Bergmann H W. Computerwissenschaft-Technik und Ihre Anwendung, Kolloquium der Chinesischen Wissenschaftler in der BRD Cowitean, 2-4 Oktober 1984, Verein der Chinesischen Wissenschaftler 6 Yinnon H, Uhlmann D R. J Non-Cryst Solids, 1983; 54: 253-275 7 Markworth A J, Glasser M L. J Appl Phys, 1983; 54: 3502-3508 8 Christian J W. The Theory of Transformations in Metals and Alloys, 2nd ed. Part I. New York: Pergamon Press, Oxford, 1965, 525 9 Altounian Z, Tu Guohua, Strom-Olsen J O. J Appl Phys, 1983; 54: 3111 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|