| Ta-Ni和Nb-Ni的熔盐电化学表面合金化及合金性质的研究 |
| 乔芝郁;PieereTaxil |
| 北京钢铁学院;法国Paul;Sabatier大学 |
|
| ELECTROCHEMICALLY SURFACE ALLOYING ON Ni WITH Ta AND Nb IN MOLTEN FLUORIDES AND PROPERTIES OF Ta-Ni AND Nb-Ni ALLOYS |
| by QIAO Zhiyu(Beijing University of Iron and Steel Technology); Pieere TAXIL (Universite Paul Sabatier; Toulouse; France)(Manuscript received 9 January; 1986; revised manuscript 3 July; 1986) |
引用本文:
乔芝郁;PieereTaxil. Ta-Ni和Nb-Ni的熔盐电化学表面合金化及合金性质的研究[J]. 金属学报, 1987, 23(2): 198-205.
,
.
ELECTROCHEMICALLY SURFACE ALLOYING ON Ni WITH Ta AND Nb IN MOLTEN FLUORIDES AND PROPERTIES OF Ta-Ni AND Nb-Ni ALLOYS[J]. Acta Metall Sin, 1987, 23(2): 198-205.
1 Taxil P, Qiao Zhiyu. J Appl Electrochem 1985; 15: 947 2 Taxil P, Qiao Zhiyu. Electrochem Soc 168th Fall Meeting Extended Abstr., Las Vegas, Nevada 85-2, 1985, 746 3 乔芝郁,在法国保尔沙巴基埃的研究报告,1984 4 Cook N C. Sci Am, 1964; 221: 38 5 Cook N C. Presented at NATO Advanced Study Institute Conference "The Science and Technology of Surface Coatings" Imperial College of Science and Technology, London, 1972 6 Weppner W, Huggins R A. Proc. on the Symp. on Electrode Materials and Process for Energy Conversion and Storage. New York: Electrochemical Society, 1977, 833 7 Weppner W, Huggins R A. J Electrochem Soc. 1977; 124: 1569 8 Weppner W, Huggins R A. J Electrochem Soc. 1978; 125: 7 9 Wen G J, Weppner W, et al. J Electrochem Soc, 1979; 126: 2258 10 Mottot Y. Doct. Etat Thesis, Paris, 1985 11 Qiao Zhiyu, Taxil P. J Appl Electrochem, 1985; 15: 259 12 Taxil P, Mahenc J. Corros Sci, 1981; 21: 31 13 Cohen U. PhD Dissertation, Stanford University, 1977 14 Taxil P. J Less-Common Met, 1985; 113: 89 15 #12 16 #12 17 Danckwerts P V. Trans Faraday Soc 1950; 46: 701 18 Jost W. Diffusion in Solids, Liquids and Gases. New York: Academic Press, 1960, 72 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|