| 合金结构钢的一种伪断口遗传 |
| 戚正风;任瑞铭 |
| 大连铁道学院;大连铁道学院 |
|
| A PSEUDO-INHERITANCE OF FRACTURE OF ALLOY STRUCTURAL STEEL |
| QI Zhengfeng; REN Ruiming (Dalian Railway Institute) (Manuscript received 15 February; 1985; revised manuscript 23 April; 1986) |
引用本文:
戚正风;任瑞铭. 合金结构钢的一种伪断口遗传[J]. 金属学报, 1987, 23(2): 158-161.
,
.
A PSEUDO-INHERITANCE OF FRACTURE OF ALLOY STRUCTURAL STEEL[J]. Acta Metall Sin, 1987, 23(2): 158-161.
1 戚正风,刘世程.大连铁道学院学报,1983;(1-2) :21 2 Ko T, Hanson D. J Iron Steel Inst 1950; 164: 51 3 赵坚.金属学报,1978;14:316 4 #12 5 #1 |
|