| In清洁表面氧吸附及早期氧化的CLS和AES研究 |
| 戴道宣;朱福荣 |
| 复旦大学表面物理实验室;复旦大学表面物理实验室 |
|
| CLS AND AES STUDIES OF OXYGEN ADSORPTION AND INITIAL OXIDATION ON CLEAN In SURFACE |
| DAI Daoxuan; ZHU Furong (Surface Physics Laboratory; Fudan University. Shanghai) (Manuscript received 4 January. 1985; revised manuscript 10 June. 1986) |
引用本文:
戴道宣;朱福荣. In清洁表面氧吸附及早期氧化的CLS和AES研究[J]. 金属学报, 1987, 23(2): 162-164.
,
.
CLS AND AES STUDIES OF OXYGEN ADSORPTION AND INITIAL OXIDATION ON CLEAN In SURFACE[J]. Acta Metall Sin, 1987, 23(2): 162-164.
Aden E H, Seymour D L, Pattinson E B. Surf Sci 1984; 141: 1 2 Wilmson C W, Kee R W. J Vac Sci Technol 1977; 14: 953 3 Ohnson O J. Chem Scr 1975; 8: 162 4 Tu C W, Schlier A R. Appl Surf Sci 1982; 11/12: 355 5 Bevolo A J, Derhvever JD, Nvack M. Sur Sci 1983; 134: 49 |
|