| Fe-Mn-C系M_s及马氏体相变驱动力的热力学计算 |
| 张鸿冰;倪乐民;徐祖耀 |
| 上海冶金专科学校;上海冶金专科学校;上海交通大学 |
|
| THERMODYNAMIC CALCULATION OF M_S AND DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS |
| ZHANG Hongbing NI Lemin (Shanghai Technical College of Metallurgy);XU Zuyao (T.Y.Hsu)(Shanghai Jiaotong University) |
引用本文:
张鸿冰;倪乐民;徐祖耀. Fe-Mn-C系M_s及马氏体相变驱动力的热力学计算[J]. 金属学报, 1987, 23(1): 42-49.
,
,
.
THERMODYNAMIC CALCULATION OF M_S AND DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS[J]. Acta Metall Sin, 1987, 23(1): 42-49.
1 Zener C.Trans AIME 1946;167:550 2 徐祖耀,金属学报,1980;16:426 3 Fisher J C.Trans AIME,1949;185:628 4 徐祖耀,金属学报,1979;15:329 5 Hsu T Y(Xu Zuyao),Chang Hongbing.Acta Metall,1984;32:343 6 Hsu T Y(XU Zuyao),J Mater Sci,1985;20:23 7 Nichol T,J,Judd G.Ansell G S.Metall Trans,1977;8A:1877 8 Kato T,Fukui S,Fujikura M,et al.Trans Iron Steel Inst Jpn,1976;16:673 9 徐祖耀,张鸿冰,罗守福,金属学报,1984;20:A151 10 Hsu T Y(Xu Zuyao),Chang Hongbing,Luo Shufu,J Mater Sci,1983;18:3206 11 Shifler G J,Bradley J R,Aaronson H I.Metall Trans,1978;9A:999 12 Zener C.Trans AIME,1955;203:619 13 Mon Yiwen,Hsu T Y(XuZuyao).Acta Metall,1986;34:325 14 Aaronson H I,Domain H A,Pound G M.Trans Metall Soc AIME 1966;236:768 15 Greninger A B.Trans ASM 1942;30:1 16 Kaufman L.Radcliffe S V,Cohen M.In:Zackey V F,Aaronson H I.eds.,Decomposition of Austenite by Diffusional Processes.Interscience Publ,1962;313 17 Andrew K W.J Iron Steel Inst,1965;203:721 18 Kung C Y,Ratmet J J.Metall Trans,1982;13A:328 19 徐祖耀,马氏体相变与马氏体,科学出版社,1981,237 20 Lobo J A,Geiger G H.Metall Trans,1976;7A:1359 21 Wada T,Wada H,Elliott J F et al.Metall Trans 1972;3:1657 22 Hultgren R,Desai P.D,Hawkins D T et al.Selected Values of Thermodynamic Properties of the Elements,Ohio:ASM,1973,171 23 Breedis J F,Kaufman L.Metall Trans,1971;2:2359 24 徐祖耀,金属学报,1980;16:420 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|