| Cu-Fe-Sn三元系合金相图 |
| 周怀营;郑建宣 |
| 广西大学物理系;广西大学物理系 |
|
| PHASE DIAGRAM OF CU-Fe-Sn TERNARY SYSTEM |
| ZHOU Huaiying ZHENG Jianxuan (Guangxi University;Nanning) |
引用本文:
周怀营;郑建宣. Cu-Fe-Sn三元系合金相图[J]. 金属学报, 1987, 23(1): 141-143.
,
.
PHASE DIAGRAM OF CU-Fe-Sn TERNARY SYSTEM[J]. Acta Metall Sin, 1987, 23(1): 141-143.