| 闪光焊灰斑的性质及其成因的研究 |
| 郑恩贵;田继丰;吴悦魁 |
| 中国科学院金属研究所;中国科学院金属研究所;沈阳铁路局 |
|
| ON THE NATURE AND ORIGIN OF FLAT-SPOT IN FLASH-WELDED JOINTS |
| ZHENG Engui TIAN Jifeng (Institute of Metal Research.Academia Sinica.Shenyang);WU Yuekui (Shenyang Railway Administration) |
引用本文:
郑恩贵;田继丰;吴悦魁. 闪光焊灰斑的性质及其成因的研究[J]. 金属学报, 1987, 23(1): 126-152.
,
,
.
ON THE NATURE AND ORIGIN OF FLAT-SPOT IN FLASH-WELDED JOINTS[J]. Acta Metall Sin, 1987, 23(1): 126-152.
1 A C,1949;386-399 2 Nippes E F.Savage W F.Grotke G.et al.Weld J,1957;36:192-216 3 Riecansky V.Lucas W.Weld Res Int,1974;4(4) :1-27 4 Wuppermann G T.Stahl Eisen,1971;91:1239-1249 5 Sullivan J F.Weld J,1971;50:213s-221s 6 Sequires I F.Br Weld J,1958;15:610-620 7 东方锅炉厂,焊接,1975;(2) :4-6 8 Welding Handbook,7th ed,1980Z |
|