| 喷雾冷却传热研究 |
| 张克强;袁伟霞;蔡开科 |
| 北京钢铁学院;北京钢铁学院;钢铁冶金专业1984年毕业生;北京钢铁学院 |
|
| SIMULATION OF HEAT TRANSFER BY WATER SPRAY COOLING DURING CONTINUOUS CASTING OF LOW CARBON STEEL |
| by ZHANG Keqiang;YUAN Weixia;CAI Kaike Beijing University of Iron and Steel Technology |
引用本文:
张克强;袁伟霞;蔡开科. 喷雾冷却传热研究[J]. 金属学报, 1985, 21(6): 77-82.
,
,
.
SIMULATION OF HEAT TRANSFER BY WATER SPRAY COOLING DURING CONTINUOUS CASTING OF LOW CARBON STEEL[J]. Acta Metall Sin, 1985, 21(6): 77-82.
1 Mizikar, E. A., Iron Steel Eng., 47 (1970) . № 6. 53. 2 Muller. H.; Jeschar, R., Arch. Eisenhuettenwes., 44 (1973) , 589. 3 Lambert. N.; Economopoulos, M., J. Iron Steel Inst., 208 (1970) , 917. 4 Bolle, L.; Moureau. J. C., Heat and Mass Transfer in Metallurgical Systems, Thesis of Seminar of ICHMT, Sept., 1979, p. 527. 5 Araki, K.; Moriyama. A.; Terada, K.; Mori. S., Trans. Iron Steel Inst. Jpn., 20(1980) . 462. 6 蔡开科;刘凤荣,金属学报,20(1984) ,B147. |
|