| Cu:Cu-Al扩散偶淬火冷却过程中的“界面逆向迁移效应” |
| 吕忆城;M.R.Notis;J.I.Goldstein |
| 上海交通大学;美国Lehigh大学;美国Lehigh大学 |
|
| “INTERFACE WITHDRAWAL EFFECTS”AT TWOPHASE INTERFACES OF Cu:Cu-Al DIFFUSION COUPLES DURING QUENCHING |
| Lü Yicheng(Y.C.Lu)Shanghai Jiaotong University;NOTIS;M.R.;GOLDSTEIN;J.I.Lehigh University.U.S.A. |
引用本文:
吕忆城;M.R.Notis;J.I.Goldstein. Cu:Cu-Al扩散偶淬火冷却过程中的“界面逆向迁移效应”[J]. 金属学报, 1985, 21(5): 67-148.
,
,
.
“INTERFACE WITHDRAWAL EFFECTS”AT TWOPHASE INTERFACES OF Cu:Cu-Al DIFFUSION COUPLES DURING QUENCHING[J]. Acta Metall Sin, 1985, 21(5): 67-148.