| 羟肟酸-黄药混合剂浮选氧化铜矿的研究与实践 |
| 周维志 |
| 广州有色金属研究院 |
|
| THE FLOTATION OF COPPER OXIDIZED ORES WITH MIXED REAGENT OF HYDROXAMATE AND XANTHATE |
| ZHOU Wetzhi Guangzhou Research Institute of Non-Ferrous Metals |
引用本文:
周维志. 羟肟酸-黄药混合剂浮选氧化铜矿的研究与实践[J]. 金属学报, 1985, 21(3): 87-93.
.
THE FLOTATION OF COPPER OXIDIZED ORES WITH MIXED REAGENT OF HYDROXAMATE AND XANTHATE[J]. Acta Metall Sin, 1985, 21(3): 87-93.
|