| Zn~(2+)离子水合数及水在TBP-ZnCl_2萃取体系中行为的核磁共振研究 |
| 俞斌;陈智;滕藤;沈其丰 |
| 清华大学化学与化工系;研究生南京化工学院;清华大学化学与化工系;清华大学化学与化工系;北京化工研究院 |
|
| THE N.M.R.STUDY OF HYDRATION NUMBER OF Zn~(2+) AND BEHAVIOUR OF WATER IN EXTRACTION |
| YU Bin;CHEN Zhi;TENG Teng Department of Chemstry and Chemical Engineering;Tsinghua University;Beijing;SHEN Qifeng Beijing Chemical Engineering Research Institute |
引用本文:
俞斌;陈智;滕藤;沈其丰. Zn~(2+)离子水合数及水在TBP-ZnCl_2萃取体系中行为的核磁共振研究[J]. 金属学报, 1985, 21(2): 81-87.
,
,
,
.
THE N.M.R.STUDY OF HYDRATION NUMBER OF Zn~(2+) AND BEHAVIOUR OF WATER IN EXTRACTION[J]. Acta Metall Sin, 1985, 21(2): 81-87.
1 Swift,T.J.;Sayre,W.G.,J.Chem.Phys.,44(1966) ,3567. 2 #12 3 #12 4 #12 5 Becker,E.D.,Spectrochim.Acta,17(1961) ,436. 6 Leonard,I.;Katzi,N.;Mason,G.W.;Peppard,D.F.,Spectrochim.Acta,34A(1978) ,51. 7 Giancotti,V.;Giordano,F.;Randaccio,L.;Ripamonti,A.,J.Chem.Soc.,(A),(1968) ,№3,757. |
|