| Y-Cu-Ni(Y≤16.7at.-%)三元系相图的室温截面 |
| 郑建宣;农亮勤 |
| 广西大学;广西民族学院 |
|
| A PART OF ROOM TEMPERATURE SECTION OF PHASE DIAGRAM OF Y-Cu-Ni(Y≤16.7 at.-%)SYSTEM |
| ZHENG Jianxuan Guangxi University;NONG Liangqin Guangxi Institute for Nationalities |
引用本文:
郑建宣;农亮勤. Y-Cu-Ni(Y≤16.7at.-%)三元系相图的室温截面[J]. 金属学报, 1985, 21(2): 88-91.
,
.
A PART OF ROOM TEMPERATURE SECTION OF PHASE DIAGRAM OF Y-Cu-Ni(Y≤16.7 at.-%)SYSTEM[J]. Acta Metall Sin, 1985, 21(2): 88-91.
1 Shaltiel,D.;Wernick,J.H.;Williams,H.J.;Peter,M.,Phys.Rev.,135(1964) ,A1358. 2 Domagula,R.,F.;Rausch,J.J.;Levinson,Do W.,Trans.ASM,53(1961) ,150. 3 Wernick,J.H.;Geller,S.,Acta Cryst.,12(1959) ,662. 4 Buschow,K.H.J.;Van Der Goot,A.S.,Acta Cryst.,B27(1971) ,1087. 5 Gschneidner,K.A.,Jr.,Rare Earth Alloys,D.Van Nostrand Company Inc.,Princeton,New Jersy,1961,p.160. 6 Chuang,Y.C.;Wu,C.H.;Chang,Y.C.,J.Less-Common Met.,84(1982) ,204. 7 Beaudry,B.J.;Daane,A.H.,Trans.Metall.Soc.AIME,218(1960) ,854. 8 Hansen,M.;Anderko,K.,Constitution of Binary Alloys,McGraw-Hill,New York,1958,p.601.- |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|