| 奥氏体不锈钢应力腐蚀和氢致开裂的机理 |
| 褚武扬;王核力;马若涛;肖纪美 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| MECHANISM OF SLOW CRACK GROWTH AND STRESS CORROSION CRACKING IN AUSTENITIC STAINLESS STEEL |
| CHU Wuyang;WANG Heli;MA Ruotao;XIAO Jimei(Chi-Mei Hsiao)Beijing University of Iron and Steel Technology |
引用本文:
褚武扬;王核力;马若涛;肖纪美. 奥氏体不锈钢应力腐蚀和氢致开裂的机理[J]. 金属学报, 1985, 21(1): 86-94.
,
,
,
.
MECHANISM OF SLOW CRACK GROWTH AND STRESS CORROSION CRACKING IN AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 1985, 21(1): 86-94.
1 Whiteman,M.B.;Troiano,A.R.,Corrosion,21(1965) ,53. 2 Eliezer,D.;Chakrapani,D.G.;Altstetter,C.J.;Pugh,E.N.,Metall.Trans.,10A(1979) ,935. 3 Singh,S.;Altstetter,C.,Metall.Trans.,13A(1982) ,1799. 4 Chu,W.Y.(褚武扬);Yao.J.(姚京);Hsiao,C.M.(肖纪美),Metall.Trans.,15A(1984) ,729. 5 姚京;褚武扬;肖纪美,金属学报,20(1984) ,A124. 6 Chu,W.Y.(褚武扬);Li,S.Q.(李世琼);Hsiao,C.M.(肖纪美);Tien,J.Z.(田中卓),Corrosion,36(1980) ,475. Chu,W.Y.(褚武扬);Liu,T.H.(刘天化);Hsiao,C.M.(肖纪美);Li,S.Q.(李世琼),Corrosion,37(1981) ,320. 7 Chu,W.Y.(褚武扬);Li,S.Q.(李世琼);Hsiao,C.M.(肖纪美);Ju,S.Y.(朱淑彦),Corrosion,37(1981) ,514. Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美);Ju,S.Y.(朱淑彦);Wang,C.(王枨),Corrosion,38(1982) ,446. 8 Chu,W.Y.(褚武扬);Wang,Y.B.(王燕斌);Hsiao,C.M.(肖纪美);Corrosion,38(1982) ,561. 9 褚武扬;肖纪美;李世琼,金属学报,17(1981) ,10. 褚武扬;肖纪美;李世琼;朱淑彦,ibid.,18(1982) ,47. 10 Theus,G.J.;Staehle,R.W.,Stress Corrosion Cracking and Hydrogen Embrittlement of Iron Base Alloy,Eds.Staehle,R.W.;Hochmann,J.,NACE,Houston,1977,p.845. 11 姚京;褚武扬;肖纪美,金属学报,19(1983) ,A445. 12 Chu,W.Y.(褚武扬);Yao,J.(姚京);Hsiao,C.M.(肖纪美),Corrosion,40(1984) ,302 13 褚武扬;林实;王枨;田中卓,断裂韧性测试,科学出版社,1979,p.158. 14 褚武扬著,氢损伤和氢致开裂,冶金工业出版社,即将出版. 15 Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美);Metall.Trans.,15A(1984) ,2087. 16 禇武扬;肖纪美;李文学;张彦国,金属学报,20(1984) ,A189. 17 褚武扬编著,断裂力学基础,科学出版社,1979,p.28. 18 Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美);Jin,L.J.(金连强);Liu,T.W.(刘天化),Scr.Metall.,17(1983) ,993. 19 乔利杰;褚武扬;肖纪美,氢在奥氏体不锈钢应力腐蚀中的作用,待发表.Y |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|