| 测算嵌镶块大小和点阵畸变中衍射线线形几何宽化的校正公式 |
| 白埃民;何崇智 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| CORRECTIONAL FORMULAE FOR X-RAY PROFILE GEOMETRIC BROADENING IN MEASUREMENT OF MOSAIC SIZE AND LATTICE DISTORTION |
| BAI Aimin; HE Chongzhi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 26 November; 1983) |
引用本文:
白埃民;何崇智. 测算嵌镶块大小和点阵畸变中衍射线线形几何宽化的校正公式[J]. 金属学报, 1984, 20(6): 471-474.
,
.
CORRECTIONAL FORMULAE FOR X-RAY PROFILE GEOMETRIC BROADENING IN MEASUREMENT OF MOSAIC SIZE AND LATTICE DISTORTION[J]. Acta Metall Sin, 1984, 20(6): 471-474.
1 #12 2 Klug, H. P.; Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous Materials, 2nd ed., Wiley, New York, 1974, p.618. 3 Jones, F. W., Proc. R. Soc., London, 166A (1938) , 16. 4 Powell, M. J. D., Computer J., 7 (1964) , 155. |
|