| LaNi_(5-x)Cu_x的还原扩散法合成及性质的研究 |
| 郑朝贵;董成;钱久信;叶于浦 |
| 北京大学化学系;北京大学化学系;北京大学化学系;北京大学化学系 |
|
| ON THE SYNTHESIS BY REDUCTION-DIFFUSION AND THE PROPERTIES OF LaNi_(5-x)Cu_x ALLOYS |
| ZHENG Chaogui; DONG Cheng; QIAN Jiuxin; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 8 September; 1983; revised manuscript 7 February; 1984) |
引用本文:
郑朝贵;董成;钱久信;叶于浦. LaNi_(5-x)Cu_x的还原扩散法合成及性质的研究[J]. 金属学报, 1984, 20(6): 458-464.
,
,
,
.
ON THE SYNTHESIS BY REDUCTION-DIFFUSION AND THE PROPERTIES OF LaNi_(5-x)Cu_x ALLOYS[J]. Acta Metall Sin, 1984, 20(6): 458-464.
1 Dwight, A. E., The Rare Earth in Modern Science and Technology, Proc. 13th Rare Earth Res. Conf. (1977) , Eds. Macarthy, G. J.; Rtyne, J. J., Plenum, New York, 1978, p. 325. 2 Van Mal, H. H., J. Less-Common Met., 35 (1974) , 65. 3 Shinar, J.; Shaltiel, D., J. Less-Common Met., 60 (1978) , 209. 4 申沣文;汪根时;张允什;宋德英;臧弢石;余素清,高等学校化学学报,1(1980) ,№2,109. 5 顾函珍;叶于浦,科学通报,12(1983) ,735. 6 钱久信;郑朝贵;张吉伟;张菊梅,全国第一届贮氢会议论文,1981. 7 #12.k |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|