| Al-Mg-Ce三元合金相图及其性能 |
| 崔忠圻;吴忍畊 |
| 哈尔滨工业大学;哈尔滨工业大学 |
|
| PHASE DIAGRAM AND PROPERTIES OF TERNARY Al-Mg-Ce ALLOYS |
| CUI Zhongqi; WU Rengeng (Harbin Institute of Technology) (Manuscript received 3 November; 1983) |
引用本文:
崔忠圻;吴忍畊. Al-Mg-Ce三元合金相图及其性能[J]. 金属学报, 1984, 20(6): 429-437.
,
.
PHASE DIAGRAM AND PROPERTIES OF TERNARY Al-Mg-Ce ALLOYS[J]. Acta Metall Sin, 1984, 20(6): 429-437.
1 大西忠一;中谷義三,轻金属,29(1979) ,21. 2 #12 3 Trehan, Y. N.; Gupte, P. K., Indian Constr. News, 10 (1961) , №10, 90. 4 #12 5 崔忠圻,哈尔滨工业大学研究生论文,1964. |
|