Please wait a minute...
金属学报  1984, Vol. 20 Issue (6): 423-428    
  论文 本期目录 | 过刊浏览 |
LaNi_xAl_y合金吸氢性能的研究
钱久信;赵黎明;郑朝贵;叶于浦
北京大学化学系;北京大学化学系;北京大学化学系;北京大学化学系
HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS
QIAN Jiuxin; ZHAO Liming; ZHENG Chaogui; YE Yupu (Department of Chemistry; Peking University. Beijing) (Manuscript received 15 September; 1983; revised manuscript 9 February; 1984)
引用本文:

钱久信;赵黎明;郑朝贵;叶于浦. LaNi_xAl_y合金吸氢性能的研究[J]. 金属学报, 1984, 20(6): 423-428.
, , , . HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS[J]. Acta Metall Sin, 1984, 20(6): 423-428.

全文: PDF(408 KB)  
摘要: 本文借助X射线衍射法确定了La-Ni-Al三元体系中以LaNi_5为基的固溶体范围。800℃时其范围为:Al<12.2wt-%, 31wt-%
Abstract:X-ray diffraction analysis was used to ascertain the LaNi_5-base solid solution range in the La-Ni-Al ternary system This range at 800℃ was found to be Al< 12.2 and 31
收稿日期: 1984-06-18     
1 Van Mal, H. H.; Buschow, K. H. J.; Miedema, A. R., J. Less-Common Met., 35 (1974) , 65.
2 Mendelsohn, M. H.; Gruen, D. M.; Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 25.
3 Achard, J. C.; Percheron-Guegan, A.; Diaz, H.; Briaucourt, F.; Demany, F., Hydrogen in Metall, Vol.2, Proc. of the 2nd Int. Congress, Held at Paris, June 1977, Behalf of the Int. Association for Hydrogen Energy, Paris, 1977, p. 1El2.
4 Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 325.+
No related articles found!