| 钛合金热稳定性研究 Ⅱ.过渡族元素在Ti_3X相形成中的行为 |
| 李东;刘羽寅 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| ON THE THERMAL STABILITY OF Ti ALLOYS Ⅱ. The Behaviour of Transition Elements in Ti_3X-Phase Formation |
| LI Dong; LIU Yuyin Sinica; Shenyang)(Manuscript received February; 1984)(Institute of Metat Research; Academia 4 November; 1983; revised manuscript 29 |
引用本文:
李东;刘羽寅. 钛合金热稳定性研究 Ⅱ.过渡族元素在Ti_3X相形成中的行为[J]. 金属学报, 1984, 20(6): 384-486.
,
.
ON THE THERMAL STABILITY OF Ti ALLOYS Ⅱ. The Behaviour of Transition Elements in Ti_3X-Phase Formation[J]. Acta Metall Sin, 1984, 20(6): 384-486.
| 1 李东;刘羽寅;万晓景,金属学报,20(1984) ,A375.屯屯屯屯屯 |
|