| Sn-Bi系凝固过程中的声发射 |
| 纪士辰;朱祖铭;王国志;李英敖;胡壮麒 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| ACOUSTIC EMISSION FROM SOLIDIFICATION OF Sn-Bi BINARY ALLOY |
| JI Shichen; ZHU Zuming; WANG Guozhi; LI Ying'ao; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 28 February; 1983) |
引用本文:
纪士辰;朱祖铭;王国志;李英敖;胡壮麒. Sn-Bi系凝固过程中的声发射[J]. 金属学报, 1984, 20(3): 237-242.
,
,
,
,
.
ACOUSTIC EMISSION FROM SOLIDIFICATION OF Sn-Bi BINARY ALLOY[J]. Acta Metall Sin, 1984, 20(3): 237-242.