| 铸钢和锻钢在水介质中应力腐蚀性能的对比研究 |
| 褚武扬;肖纪美;李文学;张彦国 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| COMPARISON OF STRESS CORROSION CRACKING BETWEEN CAST AND FORGED STEELS IN WATER |
| CHU Wuyang; XIAO Jimei (Hsiao Chi-mei); LI Wenxue; ZHANG Yanguo (Beijing University of Iron and Steel Technology) (Manuscript received 1 April; 1983) |
引用本文:
褚武扬;肖纪美;李文学;张彦国. 铸钢和锻钢在水介质中应力腐蚀性能的对比研究[J]. 金属学报, 1984, 20(3): 189-196.
,
,
,
.
COMPARISON OF STRESS CORROSION CRACKING BETWEEN CAST AND FORGED STEELS IN WATER[J]. Acta Metall Sin, 1984, 20(3): 189-196.
1 褚武扬;肖纪美;屠欢,金属热处理,(1979) ,№3,18. 2 Chu,W.Y.(褚武扬);Lu,T.W.(刘天化);Hsiao,C.M.(肖纪美);Li,S.Q.(李世琼),Corrosion,37(1981) ,320. 3 Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美);Li,S.Q.(李世琼);Ju,S.Y.(朱淑彦),Corrosion,37(1981) ,514. Chu,W.Y.(褚武扬);Li,S.Q.(李世琼);Hsiao,C.M.(肖纪美);Tien,Z.J.(田中卓),Corrosion,36(1980) .475. Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美);Ju,S.Y.(朱淑彦);Wang,C.(王枨),Corrosion,38(1982) .446. 4 Barth, C. F.; Steigcrwald, E. A.; Troiano, A. R., Corrosion, 25 (1969) , 353. ; Barth, C. F.;Troiano, A.R., Corrosion, 28(1972) , 259. 5 褚武扬;李世琼;肖纪美;王枨,金属学报,16(1980) ,179. 6 Gerberich, W. W., Hydrogen in Metal, Eds. Bernstein, I. M.; Thompson, A.W., AIME 1974, P.115. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|