| 多晶Al的循环变形 |
| 陈贤芬;林栋樑 |
| 上海交通大学;上海交通大学 |
|
| CYCLIC DEFORMATION OF ALUMINUM POLYCRYSTALS |
| CHEN Xianfeng; LIN Donglian (T. L. Lin)(Shanghai Jaiotong University) (Manuscript received 11 March; 1983; revised manuscript 14 October; 1983) |
引用本文:
陈贤芬;林栋樑. 多晶Al的循环变形[J]. 金属学报, 1984, 20(3): 169-284.
,
.
CYCLIC DEFORMATION OF ALUMINUM POLYCRYSTALS[J]. Acta Metall Sin, 1984, 20(3): 169-284.
1 Mughrabi, H.; Herz, K.; Ackerman, F., Proc. of 4th Int. Conf. on Strength of Metals and Alloys, Nancy, France, 1976, Vol.3, p.1244. 2 Mugharbi, H., Muter. Sci. Eng., 33 (1978) , 207. 3 Winter, A.T., Philos. Mag., 30 (1974) , 719. 4 Hancock, J. R.; Grosskreutz, J.C., Acta Metall., 17 (1969) , 77. 5 Kuhlmann-Wilsdorf, D., Mater. Sci. Eng., 27 (1977) , 137. 6 Mughrabi, H.; Wang, R. (王仁卉), Deformation of Polycrystals Mechanisms and Microstructures, Proc. of the 2nd Ris Int. Symp. on Metallurgy and Materials Science, Eds. Hansen, Horsewell, A.; Leffers, T.; et al., RIS National Laboratory, Roskilde, Denmark, 1981, p.87. 7 Rasmussen, K.V.; Pedersen, O.B. Proc. of 5th Int. Conf. on the Strength of Metals and Alloys, Eds. Haasen, P.; Gerald, V.; Kostorz, G., Aachen, 1979, Vol.2, p.1219. 8 Rasmussen, K.V.; Pedersen, O.B., Acta Metall., 28 (1980) , 1467. 9 Lukas, P.; Klesnil, M.,Mater. Sci. Eng., 11 (1973) , 345. 10 Figueroa, J.C.; Bhat, S.P.; de la Veaux, R.; Murzenski, S.; Lar Laird, C., Acta Metall., 29 (1981) , 1667. 11 Grosskreutz, J.C.; Mughrabi, H., Description of the Work-Hardened Structure at Low Temperature in Cyclic Deformation, in: Constitutive Equations in Plasticity, Ed. Argon, A. S., MITPress, Cambridge, Hassachusetts, 1975, p.251-326. 12 Winter, A.T.; Pedersen, O.B.; Rasmussen, K.V., Acta Metall., 29 (1981) , 735. 13 Snowden, K. U., Acta Metall., 11 (1963) , 675. 14 Grosskreutz, J.C.; Waldow, P., Acta Metall., 11 (1963) , 717. 15 Feltner, C.E., Acta Metall., 11 (1963) , 817. 16 Grosskreutz, J.C., J. Appl. Phys., 34 (1963) , 372. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|