| 稀土元素对一种Cr-Ni奥氏体钢高温蠕变断裂行为的影响 |
| 邱巨峰 |
| 冶金工业部包头冶金研究所 |
|
| INFLUENCE OF RE ADDITION ON CREEP-RUPTURE BEHAVIOUR OF A CrNi AUSTENITIC STEEL |
| by QIU Jufeng (Baotou Institute of Metallurgy; Ministry of Metallurgical Industry) (Manuscript received 15 November; 1982: revised manuscript 26 August; 1983) |
引用本文:
邱巨峰. 稀土元素对一种Cr-Ni奥氏体钢高温蠕变断裂行为的影响[J]. 金属学报, 1984, 20(2): 92-212.
.
INFLUENCE OF RE ADDITION ON CREEP-RUPTURE BEHAVIOUR OF A CrNi AUSTENITIC STEEL[J]. Acta Metall Sin, 1984, 20(2): 92-212.
1 李有柯;朱自勇;师昌绪,钢铁,(1965) ,№.11,17. 2 #12 3 #12 4 #12 5 邱巨峰;程万荣;游俊富,金属学报,17(1981) ,94. 6 Bates, J. F.; Loginow, A. W., U. S. Pat., 3523 788, August 11, 1970. or Alloy Digest, ss-253, April, 1971. 7 Perry, A.J., J. Mater. Sci., 9(1974) , 1016. 8 Briant, C. L.; Banerji, S. K., Inter. Met. Rew., 23(1978) , 164. |
|