| CrMoV钢时效前热处理对磷在晶界偏析的影响 |
| 曲哲;C.J.McMahon;Jr |
| 中国科学院金属研究所;美国Pennsylvania大学;美国Pennsylvania大学 |
|
| THE EFFECTS OF PREAGEING ON SEGREGATION OF P IN A CrMoV TURBINE ROTOR STEEL |
| by QU Zhe (Institute of Metal Research; Academia Sinica; Shenyang); McMAHON C. J.; Jr (University of Pennsylvania; U. S. A.) (Manuscript received 28 December; 1982; revised manuscript 21 September; 1983) |
引用本文:
曲哲;C.J.McMahon;Jr. CrMoV钢时效前热处理对磷在晶界偏析的影响[J]. 金属学报, 1984, 20(2): 97-214.
,
,
.
THE EFFECTS OF PREAGEING ON SEGREGATION OF P IN A CrMoV TURBINE ROTOR STEEL[J]. Acta Metall Sin, 1984, 20(2): 97-214.
1 Gould, G. C., Am. Soc. Test. Mater., Spec. Tech. Publ., №. 407, (1968) , p. 90. 2 Yu, Jin; McMahon, C. J, Jr, Metall. Trans., 11A(1980) , 277. 3 Yu, Jin; McMahon, C. J, Jr, ibid., 291. 4 Qu, Z.; Kuo, K. H., Metall. Trans., 12A(1981) , 1333. 5 Shultz, B. J.; McMahon, C. J., Jr, Am. Soc. Test. Mater., Spec. Tech. Publ., №. 449, (1972) ,p124. 6 Powers A. E., J. Iron Steer Inst., 186(1957) , 323. 7 Low, J. R., Trans. Metall. Soc. AIME, 242(1968) , 14. 8 Greaves, R. H.; Jones, J. A., J. Iron Steel Inst., 111(1925) , 231. 9 #12 10 金子秀夫;西泽泰二;玉置维照;谷藤晓男,日本金属学会志,29(1965) ,166. 11 Kalderon, D., Proc. Inst. Mech. Eng., 186(1972) , 341. 12 Baker, R. G.; Nutting, J., J. Iron Steel, Inst., 192(1959) , 257. 13 Dumoulin, Ph.; Foucalt, M.; Guttmann, M.; Palmier, M.; Wayman, M.; Biscondi, M., Met. Sci., 14(1980) , 1. 14 Qu, Z.; McMahon, C. J., Jr, Metall. Trans., 14A(1983) , 1101. 15 Mclean, D., J. Iron Steel Inst., 174(1953) , 360.j |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|