| 优势区相图的计算机研究 |
| 王乐珊;许志宏;李大年 |
| 中国科学院化工冶金研究所;中国科学院化工冶金研究所;中国科学技术情报研究所 |
|
| STUDY OF PREDOMINANCE PHASE DIAGRAM IN METALLURGY BY USING COMPUTER |
| by WANG Leshan; XU Zhihong (Institute of Chemical Metallurgy; Academia Sinica; Beijing); LI Danian (Institute of Science and Technology Information; Beljing) (Manuscript received 8 November; 1982; revised manuscript 3 May; 1983) |
引用本文:
王乐珊;许志宏;李大年. 优势区相图的计算机研究[J]. 金属学报, 1984, 20(2): 188-198.
,
,
.
STUDY OF PREDOMINANCE PHASE DIAGRAM IN METALLURGY BY USING COMPUTER[J]. Acta Metall Sin, 1984, 20(2): 188-198.
1 Linkson, P. B., Miner. Sci. Eng., 11 (1979) , 65. 2 张索林;梁植林,有色金属,34(1982) ,№2,65. 3 Linkson, P. B., Corros. Sci., 19(1979) , 613. 4 王乐珊;许志宏,化工冶金,(1980) ,№1,88. 5 Smith, J. M.; Van Ness, H. C., Introduction to Chemical Engineering Thermodynamics, McGraw-Hill, 1975, p. 415. 6 李大年;王乐珊;许志宏,计算机应用化学,1984,待发表. 7 张显鹏,第一届全国冶炼理论学术会议文集,1982,p.40. 8 魏寿昆,冶金过程热力学,上海科学技术出版社,1980,p.354.Z |
|