| 非晶合金(Fe_(0.1)Ni_(0.5)Co_(0.4))_(78)Si_8B_(14)的低温结构弛豫现象 |
| 张延忠;金慧娟 |
| 上海钢铁研究所;上海钢铁研究所 |
|
| THE PHENOMENON OF THE LOW TEMPERATURE STRUCTURAL IN AMORPHOUS ALLOY (Fe_(0.1)Ni_(0.5)Co_(0.4))_(78)Si_8 B_(14) |
| by ZHANG Yanzhong; JIN Huijuan(Shanghai Institute of Iron and Steel Research)(Manuscript received 19 March; 1983; revised manuscript 15 August; 1983) |
引用本文:
张延忠;金慧娟. 非晶合金(Fe_(0.1)Ni_(0.5)Co_(0.4))_(78)Si_8B_(14)的低温结构弛豫现象[J]. 金属学报, 1984, 20(2): 150-153.
,
.
THE PHENOMENON OF THE LOW TEMPERATURE STRUCTURAL IN AMORPHOUS ALLOY (Fe_(0.1)Ni_(0.5)Co_(0.4))_(78)Si_8 B_(14)[J]. Acta Metall Sin, 1984, 20(2): 150-153.
1 Yamada,Y.;Ohta,K.,固体物理,10(1975) ,363. 2 郭慧群;章综,物理,3(1974) ,367. 3 Egami, T., J. Appl. Phys., 50(1979) , 1564. 4 Egami, T., J. Mater. Sci., 13(1978) , 2587. 5 Ohta, K., J. Magn. Magn. Mater., 19(1980) , 165. 6 Matsuyama, T., ibid., 19(1980) , 55. 7 Chen, N. Y.; Egami, T., J. Appl. Phys., 50(1979) , 7615. 8 Allia, P., ibid., 52(1981) , 3553. 9 Egami, T., Mater. Res. Bull., 13(1978) , 557. 10 Allia, P., J. Magn. Magn. Mater., 19(1980) , 281. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|