RE对Fe-Cr-Al合金α-Al_2O_3层晶粒生长的影响 |
李碚;颜玉新 |
包头冶金研究所;包头冶金研究所 |
|
INFLUENCE OF RE ADDITION ON GRAIN GROWTH OFα-Al_2O_3 LAYER ON Fe-Cr-Al ALLOY |
by LIBei; YAN Yuxin (Baotou Research Institute of Metallurgy; Nei Monggol)(Manuscript received 1 July; 1980; revised manuscript 1 August; 1983) |
引用本文:
李碚;颜玉新. RE对Fe-Cr-Al合金α-Al_2O_3层晶粒生长的影响[J]. 金属学报, 1984, 20(2): 143-220.
,
.
INFLUENCE OF RE ADDITION ON GRAIN GROWTH OFα-Al_2O_3 LAYER ON Fe-Cr-Al ALLOY[J]. Acta Metall Sin, 1984, 20(2): 143-220.
1 李碚;骆继群,金属学报,16(1980) ,401. 2 Golightly, F. A.; Stott, F. H.; Wood, G. C., Oxid. Met., 10 (1976) , 163. 3 Giggins, C. S.; Pettit, F, S., PWA Rep. 5364, (1975) . 4 李碚;骆继群;于洪香,钢铁,16(1981) ,№9,44. 5 Mistier, R. E.; Coble, R. L., J. Am. Ceram. Soc., 54(1971) , 60. 6 永井宏;村井照幸;三谷裕康,日本金属学会志,42(1978) ,1138. 7 Felten, E. J., J. Electrochem. Soc., 108(1961) , 490. 8 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸,金属学报,17(1981) ,233. |
|