| γ-NiS加压氧化酸浸动力学的研究 |
| 方兆珩;夏光祥;陈家镛 |
| 中国科学院化工冶金研究所;中国科学院化工冶金研究所;中国科学院化工冶金研究所 |
|
| THE KINETICS OF SULPHURIC ACID LEACHING OF SYNTHETIC γ-NiS UNDER OXYGEN PRESSURE |
| FANG Zhaoheng; XIA Guangxiang; CHEN Jiayong(CHEN Chiayung)(Institute of Chemical Metallurgy; Academia Sinica; Beijing)(Manuscript received 21 November; 1982; revised manuscript 4 May; 1983) |
引用本文:
方兆珩;夏光祥;陈家镛. γ-NiS加压氧化酸浸动力学的研究[J]. 金属学报, 1984, 20(1): 123-130.
,
,
.
THE KINETICS OF SULPHURIC ACID LEACHING OF SYNTHETIC γ-NiS UNDER OXYGEN PRESSURE[J]. Acta Metall Sin, 1984, 20(1): 123-130.
1 Llanos, Z.R.; Queneau, P.B.; Richard, R.S., CIM Bull., 67 (1974) , No. 742, 17. 2 夏光祥;张福鑫;张道权,高冰镍浸取动力学的研究,1980,未发表资料. 3 Richard, W.H., Eng. Min. J., 178 (1977) , No. 5, 76. 4 #12 5 #12 6 Nicolic, C., Diss. Abstr. Int., Sect. B, 40 (1979) , 880. 7 Hass, L.A.; Schluter, R.B.; Mahan, W.M., Eng. Min. J., 178 (1977) , No. 4, 80. |
|