| 一个精确的压扁弧长数学模型 |
| 苏逢西;蒋金梅;陈田青 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| AN ACCURATE MATHEMATICAL MODEL OF ROLL FLATTENED ARC LENGTH |
| SU Fengxi; JIANG Jinmei; CHEN Tianqen (Beijing University of Iron and Steel Technology)(Manuscript received 7 January; 1982; revised manuscript 27 May; 1983) |
引用本文:
苏逢西;蒋金梅;陈田青. 一个精确的压扁弧长数学模型[J]. 金属学报, 1984, 20(1): 131-140.
,
,
.
AN ACCURATE MATHEMATICAL MODEL OF ROLL FLATTENED ARC LENGTH[J]. Acta Metall Sin, 1984, 20(1): 131-140.
1 Hitchcock, J. H., Roll Neck Bearings, Appcndic I ASME Report of Special Research Commitce, 1935. 2 苏逢西;葆鸿熙,板带轧制压扁弧长的研究,北京钢铁学院研究生毕业论文,1981. 3 Bland, D.R.; Ford, H., J. Iron Steel Inst., 171 (1952) , 245. 4 #12 5 Stone, M.D., Iron Steel Eng., 30 (1953) , No. 2, 61. 6 Hill, R., The Mathematical Theory of Plasticity, Clarendon Pr., Oxford, 1950, p. 199. 7 Whitton, P.W.; Ford, H., Proc. Inst. Mech. Eng., 169 (1955) , 123.u |
|