| Fe_5Co_(73)Si_(10)B_(12)非晶态合金磁各向异性与旋转磁场热处理效应 |
| 官可洪;孙庭烈;李东辉 |
| 东北工学院;东北工学院;东北工学院 |
|
| EFFECT OF ROTATIONAL FIELD ANNEALING ON MAGNETIC ANISOTROPY OF Fe_5Co_(73)Si_(10)B_(12) AMORPHOUS ALLOY |
| GUAN Kehong; SUN Tinglie; LI Donghui (Northeast Institute of Technology; Shenyang) |
引用本文:
官可洪;孙庭烈;李东辉. Fe_5Co_(73)Si_(10)B_(12)非晶态合金磁各向异性与旋转磁场热处理效应[J]. 金属学报, 1983, 19(5): 53-57.
,
,
.
EFFECT OF ROTATIONAL FIELD ANNEALING ON MAGNETIC ANISOTROPY OF Fe_5Co_(73)Si_(10)B_(12) AMORPHOUS ALLOY[J]. Acta Metall Sin, 1983, 19(5): 53-57.
1 Hiroaki Morita; Hiroyasu Fujimoro; Yoshihisa Obi, Jpn. J. Appl. Phys., 18 (1979) , 683. 2 Hiroyasu Fujimori; Tsuyoshi Masumoto, Suppement to Sci Rep., The Research Institute for Iron, Steel and Other Metals, Tohoku University, Sendai, Jpn., 1978, p. 181. 3 Hiroyasu Fujimori, Magnetic Anisotropy, Ed. Luborsky (unpublished). 4 Tsunashima, S.; Maehata, Y.; Uchiyama, S., IEEE Trans. Magn., MAG-17 (1981) , 3073 |
|