微量硫对高速钢热塑性的影响
罗迪;邢国华;邹惠良
冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;上海测试技术研究所
EFFECT OF TRACE SULPHUR ON HOT PLASTICITY OF HIGH SPEED STEELS
by LUO Di; XING Guohua (Central Iron and Steel Research Institute. Ministry of Metallurgical Industry; Beijing); ZOU Huiliang (Shanghai Institute of Test Technics) (Manuscript received 20 January; 1982; revised manuscript 3 January; 1983)
引用本文:

罗迪;邢国华;邹惠良. 微量硫对高速钢热塑性的影响[J]. 金属学报, 1983, 19(4): 117-120.
, , . EFFECT OF TRACE SULPHUR ON HOT PLASTICITY OF HIGH SPEED STEELS[J]. Acta Metall Sin, 1983, 19(4): 117-120.

全文: PDF(283 KB)  
摘要: 本文研究了微量硫对W14Cr4VMn高速钢热塑性的影响:热扭转实验证实微最硫仍能危害钢的热塑性;Auger能谱仪实验发现,即使钢中的硫含量降低到0.002wt-%时,硫仍偏聚在晶界上。本文讨论了硫偏聚和微量硫危害热塑性的原因。
Abstract:The effect of trace S on the hot plasticity of high speed steels has been examined. It was shown that the S content in W14Cr4VMn steel decreased from 0.01% down to a possible lowest limit of 0.002% the number of cycles of the hot torsion test increases about 20% under 950-1150℃. This indicates that the hot plasticity of the high speed steels may be deteriorated even if a trace S contained. AES was observed that the S segregation occurs along the austenite grain boundaries. The reason of the S segregation and its deterioration on the hot plasticity of the steels has also been discussed.
收稿日期: 1983-04-18     
1 日本铁鋼协会编,铁鋼制造法,丸善株式会社,1972,p.17.
2 冶金工业部钢铁研究总院,大连钢厂,未公开发表材料,(1979) .
3 罗迪;邢国华;沈汝美;靳达申,待发表.
4 Seah, M. P.; Hondros, E. D., Proc. R. Soc. Lond., A335 (1973) , 191.
5 Helms, C. R., Interfacial Segregation, Eds. W. C. Johnson; J. M. Blakely, ASM, Ohio, 1979, p.215
6 渡辺利光;山本広一;南雲道彦;上野正勝;铁鋼,61(1975) ,S730.
7 McLean,D.,金属中的晶粒间界、杨顺华译,科学出版社,1965,p.101.6
No related articles found!