| 熔体过热对Al-Cu合金定向凝固某些特性的影响 |
| 毛协民;傅恒志;史正兴;刘慧铭 |
| 西北工业大学;西北工业大学;西北工业大学;西北工业大学 |
|
| EFFECT OF MELT SUPERHEAT ON DIRECTIONAL SOLIDIFICATION PROPERTIES OF Al-Cu ALLOY |
| by MAO Xiemin; FU Hengzhi; SHI Zhengxing; LIU Huiming (North-Western Polytechnical University. Xi'an ) |
引用本文:
毛协民;傅恒志;史正兴;刘慧铭. 熔体过热对Al-Cu合金定向凝固某些特性的影响[J]. 金属学报, 1983, 19(3): 84-90.
,
,
,
.
EFFECT OF MELT SUPERHEAT ON DIRECTIONAL SOLIDIFICATION PROPERTIES OF Al-Cu ALLOY[J]. Acta Metall Sin, 1983, 19(3): 84-90.
1 Tiller, W. A.; Jackson, W. A., Acta Metall., 1 (1953) , 428. 2 Chalmers, B., Principles of Solidiflcation, Wiley, New York 1964, p.158. 3 Turnbull, D., J. Chem. Phys., 18 (1950) , 198. 4 #12 5 Metals Handbook, 8th ed. Vol. 8, ASM, 1973. p.78. 6 Flemings, M. C., Solidification Processing, McGraw Hill, New York, 1974. p.78.D |
|