| Fe-Cu-C和Fe-Cu-Co-C熔体的热力学性质 |
| 彭瑞伍;汪光裕;张俊岳 |
| 中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所 |
|
| THERMODYNAMIC PROPERTIES OF Fe-Cu-C AND Fe-Cu-Co-C MELTS |
| by PENG Ruiwu; WANG Guangyu; ZHANG Junyue (Shanghai Institute of Metallurgy; Academia Sinica) |
引用本文:
彭瑞伍;汪光裕;张俊岳. Fe-Cu-C和Fe-Cu-Co-C熔体的热力学性质[J]. 金属学报, 1983, 19(3): 77-83.
,
,
.
THERMODYNAMIC PROPERTIES OF Fe-Cu-C AND Fe-Cu-Co-C MELTS[J]. Acta Metall Sin, 1983, 19(3): 77-83.
1 Iwase, K., Okamoto, M., Amemiya, T.; Sci. Rep. Tohoku Imp. Univ., 26 (1937) , 618. 2 Koros, J.; Chipman, J., Trans. AIME, 206 (1956) , 1102. 3 Schenck, H., Arch. Eisenhuettenwes., 32 (1961) , 123. 4 彭瑞伍,邹元爔,金属学报,6(1963) ,111. 5 Mathien, G., Scr. Metall., 7 (1973) , 421. 6 Morris, J. P.; Zellans, G. R., Trans. AIME, 206 (1956) , 1086. 7 Foo, E. H.; Lupis, C. H. P., Metall. Trans., 3 (1972) , 2125. 8 Lupis, C. H. P., Metall. Trans., 5 (1974) , 1919. 9 彭瑞伍;汪光裕;张俊岳,待发表. 10 魏寿昆,冶金过程热力学,上海科技出版社,1980,p.231.a |
|