| Ni-Fe-Cr-Nb合金中δ相的电子衍射分析 |
| 李玉清;刘锦岩 |
| 大冶钢厂钢铁研究所;大冶钢厂钢铁研究所 |
|
| AN ELECTRON DIFFRACTION ANALYSIS OF δ-PHASE IN A Ni-Fe-Cr-Nb ALLOY |
| by LI Yuqing; LIU Jingyan (Research Institute of Daye Steel Works) |
引用本文:
李玉清;刘锦岩. Ni-Fe-Cr-Nb合金中δ相的电子衍射分析[J]. 金属学报, 1983, 19(3): 44-53.
,
.
AN ELECTRON DIFFRACTION ANALYSIS OF δ-PHASE IN A Ni-Fe-Cr-Nb ALLOY[J]. Acta Metall Sin, 1983, 19(3): 44-53.
1 Kirman, I.; Warrington, D. H., Metall. Trans., 1 (1970) , 2667. 2 李玉清;刘锦岩,金属学报,16(1980) ,245. 3 Kirman, I., J. Iron Steel Inst., 207 (1969) , 1612. 4 Frantz, C.; Gantols, M., The Microstrueture and Design of Alloys, Proc. 3rd Int. Conf. on the Strength of Metals and Alloys, Vol. 1, Cambridge, England, 1973, p. 331. 5 #12 |
|