| 高合金化镍基变形高温合金中弯曲晶界的初步研究 |
| 仲增墉;马培立;陈淦生;张俊明;李凤周;田树森 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;抚顺钢厂;抚顺钢厂;抚顺钢厂 |
|
| A STUDY OF ZIGZAG GRAIN BOUNDARY IN HIGH ALLOYED WROUGHT NICKEL-BASE SUPERALLOY |
| by ZHONG Zengyong; MA Peili; CHEN Gansheng (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); ZHANG Junming; LI Fengzhou; TIAN Shushen (Fushun Steel Works) |
引用本文:
仲增墉;马培立;陈淦生;张俊明;李凤周;田树森. 高合金化镍基变形高温合金中弯曲晶界的初步研究[J]. 金属学报, 1983, 19(3): 54-154.
,
,
,
,
,
.
A STUDY OF ZIGZAG GRAIN BOUNDARY IN HIGH ALLOYED WROUGHT NICKEL-BASE SUPERALLOY[J]. Acta Metall Sin, 1983, 19(3): 54-154.
1 Decker, R. F., Climax Molybdenum Company Symposium, Zurich 1969, p. 165. 2 Decker, R. F.; Sims, C. T., The Superalloys, Eds. Sims, C. T.; Hagel, W. C., John Wiley & Sons, 1972, p. 33. 3 Miyagawa, O.; Yamamoto, M.; Kobayshi, M., Superalloys: Metallurgy and Manufacture, Proc. of 3rd Int. Symp. on Superalloys, Eds. Kear, B. H.; Muzyka, D. R.; Tien, J. K. et al., Claitot's Publ., Baton Rouge, Louisiana, 1976, p. 245. 4 British Standard, BS HR 4, (1972) . 5 仲增墉,镍铬钴基变形高温合金中弯曲晶界的研究,钢铁研究总院,1980年学术年会论文摘要(下),p.165. 6 Lorson, J. N.; Floreen, S. F., Metall. Trans., 8A (1977) , 51. 7 #12b |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|