| 沉淀硬化镍基高温合金中γ′相体积百分数的计算表达式 |
| 杨洪才 |
| 东北工学院 |
|
| CALCULATIONAL FORMULATION FOR VOLUME PERCENT OF γ′-PHASE IN PRECIPITATION HARDENING Ni-BASE SUPERALLOYS |
| YANG Hongcai (Northeast Institute of Technology; Shenyang) |
引用本文:
杨洪才. 沉淀硬化镍基高温合金中γ′相体积百分数的计算表达式[J]. 金属学报, 1983, 19(2): 134-138.
.
CALCULATIONAL FORMULATION FOR VOLUME PERCENT OF γ′-PHASE IN PRECIPITATION HARDENING Ni-BASE SUPERALLOYS[J]. Acta Metall Sin, 1983, 19(2): 134-138.