| 镍基高温合金真空电弧重熔过程中Mg挥发的动力学 |
| 傅杰;王惠;王迪;陈恩普 |
| 北京钢铁学院;北京钢铁学院;长城钢厂三分厂;长城钢厂三分厂 |
|
| KINETICS OF Mg EVAPORATION DURING VAR OF A Ni-BASE SUPERALLOY |
| FU Jie; WANG Hui; WANG Di (Beijing University of Iron and Steel Technology); CHEN Enpu (Changcheng Steel Works; №3 Branch in Jiangyou; Sichuan) |
引用本文:
傅杰;王惠;王迪;陈恩普. 镍基高温合金真空电弧重熔过程中Mg挥发的动力学[J]. 金属学报, 1983, 19(2): 126-133.
,
,
,
.
KINETICS OF Mg EVAPORATION DURING VAR OF A Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1983, 19(2): 126-133.
1 #12 2 #12 3 #12 4 #12 5 #12 6 Debarbadillo, J. J., Superalloys, Metallurgy and Manufacture, Proceedings of the Third International Symposium, Eds. Keas, B. H. et al., Baton Rouge, Claitor's Pub. Division 1976, p. 95. 7 #12 8 #12 9 #12 10 Johnson. E. W., J. Met., 12 (1960) . 850. 11 曲英,炼钢学原理,冶金工业出版社,1980,p.74. |
|