| 16Mn钢疲劳裂纹扩展速率的研究 |
| 童志深;侯耀永;李明奇;蒋生蕊 |
| 兰州大学;兰州大学;兰州大学;兰州大学 |
|
| INVESTIGATION OF FATIGUE CRACK GROWTH RATE FOR STEEL 16Mn |
| Tong Zhishen; Hou Yaoyong; Li Mingqi; Jiang Shengrui (Lanzhou University) |
引用本文:
童志深;侯耀永;李明奇;蒋生蕊. 16Mn钢疲劳裂纹扩展速率的研究[J]. 金属学报, 1982, 18(5): 618-626.
,
,
,
.
INVESTIGATION OF FATIGUE CRACK GROWTH RATE FOR STEEL 16Mn[J]. Acta Metall Sin, 1982, 18(5): 618-626.
1 Coffin, L. F., Jr., Am. Soc. Test. Mater., Spec. Tech. Publ., № 520,(1973) , p. 5. 2 蔡其巩,金属学报,12(1976) ,45. 3 Dowling, N. E., Am. Soc. Test. Mater, Spec. Tech. Publ., № 601,(1976) , p. 19. 4 申辉旺;邓其源;蔡其巩,未发表资料,1974. 5 陈篪;姚蘅;邓枝生;庄韬;邓其源,金属学报,11(1978) ,174. 6 Mowbray, D. F., Am. Soc. Test. Mater., Spec. Tech. Publ., № 601,(1976) , p. 33. 7 兰州化工机械研究所,未发表资料,1976. |
|